. 2009 Jun 17;4(10):1159–1165. doi: 10.1007/s11671-009-9375-x

Figure 1.

Figure 1

CdS nanorods synthesized in TOP solution (40 mg cadmium acetate in 3 mL TOP and 24 mg S powder in 1 mL TOP at 260 °C for reaction 4 h): TEM image (a), HRTEM image (b), length (c) and width (d) distribution histograms of the nanorods