Skip to main content
. 2009 Jul 16;4(10):1247–1253. doi: 10.1007/s11671-009-9388-5

Figure 3.

Figure 3

aFrequency changes during LbL chitosan-HAP build-up: 1-Cht deposition, 2-rinsing, 3-H AP deposition and 4-rinsing.bDissipation changes during LbL chitosan-HAP build-up: 1-Cht deposition, 2-rinsing, 3-H AP deposition, and 4-rinsing. The 5th (squares), 7th (circles) and 9th (triangles) overtones are represented.cChange in the film’s thickness during LbL build-up: cht (squares) and HAP (circles)