Skip to main content
. 2009 May 31;4(9):1021–1028. doi: 10.1007/s11671-009-9351-5

Figure 1.

Figure 1

ESEM images of a template before and after the complete removal of the oxide barrier layer from the pore bottom tips.aCross-section of an AAO film before the removal of alumina barrier layer;bMagnified view of the area marked inawith awhite rectangle;cPore bottom detail on which we can see how the pore bottoms are opened as a whole after the process described has been carried out (thewhite arrowheadsindicate the pore bottom tips)