Fig. 5.

Fig. 5

A graph shows the root mean square error and standard deviation in lateral resection (mm) measurement of seven of the alloys: titanium; cobalt-chrome; 304 and 316 stainless steels; 260 brass; 6061 aluminum; and 110 copper, respectively. Although some metals show little effect, these are very influential in inducing errors.