Skip to main content
. 2010 May 28;5(8):1333–1339. doi: 10.1007/s11671-010-9649-3

Figure 2.

Figure 2

SEM images of ZnO nanostructures synthesized on FTO-coated glass substrates after a 30, b 80, and c 100 min at the furnace temperature of 950°C, 760 Torr, and Ar flow rate of 70 sccm