Skip to main content
. 2010 May 28;5(8):1333–1339. doi: 10.1007/s11671-010-9649-3

Figure 4.

Figure 4

SEM images of ZnO nanostructures synthesized at a 910, b 930, c 940, d 950, and e 1,000°C for 100 min with Ar flow rate of 70 sccm at 760 Torr