Skip to main content
. Author manuscript; available in PMC: 2011 Aug 1.
Published in final edited form as: J Biomed Mater Res B Appl Biomater. 2010 Aug;94(2):447–454. doi: 10.1002/jbm.b.31674

Figure 5.

Figure 5

A specimen (0.00005:1 polybutadiene/silica) fractured at 1mm/min. Note the cracks originating at aggregate equators, indicating a brittle mode of deformation.