Hot Melt Extrusion Manufacturing Conditions and Resulting Potency Values

Polymer Particle size Temperature (°C) Screw speed (rpm) Recirculation time (min) Recovery (%) Impurities (%)
Eudragit® L100-55 Unmicronized 140 300 2 22.7 ± 0.5 55.9
Eudragit® L100-55 Micronized 140 300 0 69.1 ± 0.5 17.3
HPMCAS Unmicronized 170 300 2 70.9 ± 0.3 10.2
HPMCAS Micronized 170 300 0 78.4 ± 0.1 8.9