Table 1. Measurement of apparent Young’s modulus (MPa) of inner limiting membranes from wildtype, POMGnT1 knockout and Largemyd mouse retinas.
Sample # | Wildtype | POMGnT1 knockout | Largemyd |
---|---|---|---|
1 |
4.11±0.90 |
2.83±0.95 |
1.66±0.56 |
2 |
4.01±1.02 |
2.75±1.02 |
1.90±0.93 |
3 |
3.76±1.14 |
3.10±0.84 |
1.69±0.49 |
4 | 4.46±1.41 | 2.59±0.79 | 1.46±0.54 |
Elasticity was measured at 100 random locations from each of the four inner limiting membrane (ILM) samples of every genotype. Means±standard deviations were then calculated.