Figure 6.

Figure 6

Electropherograms for the three dendrimer classes obtained using pH 9.1 100 mM borate/lithium buffer (left) and using pH 6.9 50 mM phosphate/lithium buffer (right). All traces were obtained in positive-to-negative polarity, except traces for triazine dendrimers using borate buffer, which were obtained in negative-to-positive polarity. The absorbance scale (Abs) is in milli-absorbance units (mAU) recorded at a 214 nm detection wavelength. Effective mobility scale (μeff) is in “× 10−5 cm2/V · s” units.