Skip to main content
. Author manuscript; available in PMC: 2010 Aug 23.
Published in final edited form as: Int J Pharm. 2002 Sep 5;244(1-2):9–19. doi: 10.1016/s0378-5173(02)00297-1

Fig. 6.

Fig. 6

In vitro release isotherms of naltrexone-loaded hydrolyzable crosslinked PEO–MMA nanoparticles prepared at different weight ratios of PEO–MMA (■:1/1; ▲: 1/4). Standard deviation ε (0.28; 3.52).