Skip to main content
. 2010 Apr 19;16(8):2519–2527. doi: 10.1089/ten.tea.2009.0815

FIG. 1.

FIG. 1.

The elastic modulus of PEGDMA hydrogels can be controlled by varying the monomer and crosslinker concentration. (A) PEGDMA concentration was varied from 10% to 90%, with photoinitiator-crosslinker concentration at 0.1%. (B) Photoinitiator-crosslinker was varied from 0.04% to 0.8% (w/v), with PEGDMA concentration constant at 90%. Bars indicate SD. PEGDMA, poly(ethylene glycol) dimethacrylate; SD, standard deviation.