Fig. 5.

Fig. 5

Scanning electron micrographs of 3-layer composites cross-sectioned into individual element resonators and examined for any misalignment of the individual piezoceramic layers and epoxy bond layers between the layers. A range of misalignments and bond layers was observed, ranging from (a) very good: 5-μm misalignment and no discernable bond layer, to (b) poor: 30-μm misalignment and 6-μm bond layer.