Skip to main content
. 2010 Jul 7;7(Suppl 5):S559–S579. doi: 10.1098/rsif.2010.0120.focus

Figure 11.

Figure 11.

(a) The average percentage of clearly detectable units and (b) the average SNRs recorded from various modifications of the electrodes including unmodified electrode (control), 30 µm of HG-coated electrode (HG), PEDOT-deposited electrode (PEDOT), PEDOT deposition on the electrode sites under 30 µm HG coating (HG + PEDOT). Asterisks denote significance between HG and HG + PEDOT (Kim et al. 2009).