Bruker SMART CCD area-detector diffractometer 4078 independent reflections
Radiation source: fine-focus sealed tube 3703 reflections with I > 2σ(I)
graphite Rint = 0.037
φ and ω scans θmax = 30.5°, θmin = 2.9°
Absorption correction: multi-scan (SADABS; Bruker, 2004) h = −34→34
Tmin = 0.671, Tmax = 0.846 k = −18→18
33484 measured reflections l = −25→25