Table 1.

Population doubling time (PDT) and colony forming unit-fibroblast (CFU-F) results of GNT-labeled MSCs

Cells PDT*
(h)
Plating Density
(cells/well)
CFU-F*
After 7 Days
Unlabeled 9.31 1000 252 ± 11
GNT-Labeled 7.36 1000 319 ± 9
*