SEMs of BDP produced by RESS using nozzle diameters of a 254 µm, b 762 µm, and c 1,016 µm. The experimental conditions were T mix = 40 °C, P mix = 3,000 psi, Nozzle length = 3 cm, y BDP = 2.50 × 10−3, [MeOH] = 5mol%