Table 1.
Composition of K2HPO4 solutions with varying K4P2O7 concentration used in these experiments for converting calcium–lithium–borate (CaLB3–15) glass particles to a calcium phosphate material
| K2HPO4 (M) | 0.25 | 0.25 | 0.25 | 0.25 |
| K4P2O7 (M) | 0 | 0.001 | 0.01 | 0.1 |
| Reaction time (h) | 72 | 96 | 240 | 672 |
The total reaction time for each composition is also shown