Fig. 5.

Fig. 5

Optical microscope photomicrographs of metal specimens after shear bond strength test (× 200). a. CS, b. CM, c. CC, d. CR e. TS, f. TM, g. TT, h. TC. Adhesive failure was observed in all specimens. It was observed that some resin fragments were remained on the surface of all specimens.