TABLE III.
Young Modulus† (MPa) |
||
4 Weeks | 8 Weeks | |
Group 1 (primary repair) | 7.2 ± 3.8 | 3.79 ± 2.1 |
Group 2 (primary repair and augmentation) | 4.0 ± 0.5 | 48.6 ± 9.5 |
The strain rate was 2% per second. The values are given as the mean and the standard deviation. †A significant increase in biomechanical properties was demonstrated between the four-week and eight-week results for Group 2 and between Group 1 and Group 2 at eight weeks (p < 0.05).