Published in final edited form as: Biomacromolecules. 2010 Nov 8;11(12):3219–3227. doi: 10.1021/bm100469w

Fig. 4.

Fig. 4

Fig. 4

SEM Images of as-spun (A), MeOH- (B), GTA- (C), and MeOH-GTA-treated (D) SELP-47K fibrous scaffolds electrospun from a 150 mg/mL protein solution. Scale bars: 5 μm.