Skip to main content
. Author manuscript; available in PMC: 2011 Nov 15.
Published in final edited form as: Anal Chem. 2010 Oct 21;82(22):9211–9220. doi: 10.1021/ac102262m

Figure 1.

Figure 1

SEM photograms of bare gold-covered substrate (a) and calcinated substrates fabricated with different methods: 8 layers of silicate fabricated with water washing between deposition of each polyelectrolytes (b); 4 layers of silicate fabricated without water washing (c); 8 layers of silicate fabricated without water washing (d). Amplification is ×1000. The insert pictures show substrates with 10,000-fold amplification. The scale bar represents 2 µm.