Skip to main content
. Author manuscript; available in PMC: 2012 Feb 3.
Published in final edited form as: J Biomech. 2010 Oct 27;44(3):413–418. doi: 10.1016/j.jbiomech.2010.10.001

2.

2

Representative meniscal attachment A) prior to initiation of test, and B) immediately following mid-substance failure of specimen. White lines indicate where ink lines were placed to track strain. Failure of specimen can be seen tearing midsubstance with no appearance of lines placed just below the grip face, indicating no slippage during testing.