Skip to main content
. Author manuscript; available in PMC: 2011 Feb 16.
Published in final edited form as: Langmuir. 2010 Feb 16;26(4):2659–2664. doi: 10.1021/la902920n

Figure 2.

Figure 2

Contact angle measurements of BisGMA:TEGDMA disks and the substrates on which they were prepared (Arg disks were prepared with no opposing substrate). * indicates a significant difference (p ≤ 0.05) for disks compared to the Unt disks. Bar heights are the averages (n ≥ 16), and error bars represent one standard uncertainty (1 σ).