Figure 9.

Figure 9

(a) charge storage with time (40wt% uptake) under different applied voltage step (10mV to 4V). (b) storage of double layer charge and diffusion charge under different applied voltage step. The inset graph is the charge ratio (QDL/QDiff) as a function of applied voltage step.