TABLE I.
Sample | Measured property |
|||
---|---|---|---|---|
Pr (μC/cm2) | Ec (kV/cm) | εr at 1 kHz | tan δ at 1 kHz | |
KNN/BNT (650°C) | 10.1 | 68 | 698 | 0.031 |
KNN/BNT (700°C) | 12.8 | 71 | 733 | 0.028 |
KNN/BNT (750°C) | 23.6 | 108 | 848 | 0.029 |
BNT (750°C) | 34.2 | 143 | 900 | 0.033 |
KNN [23] | 16.4 | 42 | — | — |
Soft doped PZT [12] | 15 | 23 | 900 | — |
PZT 52/48 [13], [22] | 16–37 | 40–43 | 680–1250 | 0.040 |