FITC- Dextran Molecular Weight: Adjusted R2 Deff [mm2/hr] M [mg] % Mass Loading Encapsulated
Untreated Films 4 kDa 0.989 ± 0.001 1.706E-03 ± 1.015E-04 3.976 ± 0.905 15.8 ± 4.3
10 kDa 0.999 ± 0.001 1.481E-03 ± 7.922E-05 2.450 ± 0.841 39.4 ± 6.9
20 kDa 0.995 ± 0.002 1.260E-03 ± 9.247E-05 1.880 ± 0.344 52.3 ± 2.9
40 kDa 0.993 ± 0.005 5.016E-04 ± 9.223E-05 0.568 ± 0.254 83.2 ± 6.3
MeOH Treated Films 4 kDa 0.993 ±0.001 7.425E-04 ±2.724E-05 3.756 ±0.656 15.4 ±1.1
10 kDa 0.999 ±0.001 6.337E-04 ±5.634E-05 3.047 ±0.344 23.3 ±6.3
20 kDa 0.991 ±0.003 4.712E-04 ±6.571E-05 2.115 ±0.069 34.6 ±6.6
40 kDa 0.995 ± 0.000 1.065E-04 ± 5.158E-05 1.634 ± 0.738 69.4 ± 11.5