Table 3.

Bond strengths of four adhesives when treated with and without mucin under different conditions.

Adhesive Without Mucin With Mucin
Control S SA SW S SA SW
SEB 52.9 (7.3)A 51.8 (11.3)A 19.7 (2.2)G 11.1 (3.7) 57.1 (8.8) 19.9(6.0)B,G 21.5(4.0)B,f
S3 34.3 (7.8) 26.9 (5.7) 12.9 (1.4) 30.5 (4.5) 20.0 (5.0) 16.6 (3.9)e 44.3 (9.8)
SBP 48.3 (8.8) 0.0 43.4 (6.4)C 42.4 (6.4)C 0.0 36.2 (10.6)D 35.9 (7.1)D
P&BNT 60.3 (13.3) 0.0 0.0 35.3 (5.3) 0.0 18.5 (5.6)e 22.4 (7.0)f

Means with standard deviations in parentheses (n=9) of bond strength (MPa). Fisher's PLSD intervals (p<0.05) for comparisons of means between mucin and no mucin, among adhesives, and among conditions were 1.6, 2.3 and 2.3 MPa, respectively. Means with the same superscripted letters are statistically the same (upper case describes the rows and lower case describes the columns).