Figure 3.

Figure 3

Representative gelation times of crosslinked copolymer 1 (PPF700-co-PCL530R0.3) using three different accelerator amounts: 0.5 (◇), 0.25 (□) and 0.125 (Δ) wt % of DMT/copolymer.