Size of popcorn shape gold nanoparticle before and after conjugation with aptamer and antibody

Material Hydrodynamic Diameter
Only popcorn shape gold nanoparticle 28 nm ± 2 nm
A9 aptamers conjugated popcorn shape gold nanoparticle 40 nm ± 2 nm
Anti PSMA antibody conjugated popcorn shape gold nanoparticle 44 ± 2 nm
Multifunctional popcorn shape gold nanoparticle 43 ± 3 nm