Skip to main content
. Author manuscript; available in PMC: 2012 May 1.
Published in final edited form as: Biomaterials. 2011 Feb 20;32(14):3654–3665. doi: 10.1016/j.biomaterials.2011.01.068

Fig. 3.

Fig. 3

Representative size distributions determined by DLS (a) and AFM images (b, c) of C60-POx complexes: (a, b) C60-PEtOx; (a, c) C60-P(EtOx-co-BuOx). For AFM, C60-polymer complexes were deposited on the APS mica. Concentration of the complexes is 100 μM in C60.