. 2011 May 9;4(5):857–868. doi: 10.3390/ma4050857

Figure 8.

Figure 8

(a) Representative scratch track of M1, M4, and NCD samples tested on Ti-6Al-4V substrates; (b) Higher magnification of NCD sample showing forward tensile cracking attributed to cohesive failure in coating; (c) Sample data output for NCD coated sample.