Skip to main content
. Author manuscript; available in PMC: 2012 Mar 8.
Published in final edited form as: Chem Mater. 2011 Mar 8;23(5):1130–1135. doi: 10.1021/cm1024487

Table 1.

Table representing the concentration of Ac-DOPA4-mPEG and metal salt, the metal-DOPA ratio, the surface plasmon resonance (SPR) center wavelength, and the nanoparticle size determined by TEM of metal nanoparticle samples.

[Ac-DOPA4-mPEG] (μM) [Au] (μM) [Ag] (μM) [M]/[DOPA] SPR λ (nm) Size (nm)
370 107 0 0.0723 525 10.4 ± 6.7
370 427 0 0.289 547 38.7 ± 5.5
370 625 0 0.423 559 68 ± 18
370 1970 0 1.33 ND N/A
370 0 107 0.0723 415 16.9 ± 2.4