Published in final edited form as: Dent Mater. 2011 Apr 22;27(8):762–769. doi: 10.1016/j.dental.2011.03.016

Figure 2.

Figure 2

Mechanical properties of NACP nanocomposites. (A) Flexural strength before immersion. (B) Elastic modulus before immersion. (C) Flexural strength after 1 d immersion at pH 7. (B) Elastic modulus after 1 d immersion at pH 7. The properties for the NACP composites are plotted vs. NACP filler level. The two commercial materials are near the right axis as controls. Each value is the mean of six measurement, with the error bar showing one standard deviation (mean ± sd; n = 6).