Skip to main content
. 2011 Jul 6;101(1):128–133. doi: 10.1016/j.bpj.2011.05.054

Figure 5.

Figure 5

(a) NR measurements of polymer-DPPE (upper two NR profiles) and polymer-DPPC (lower two profiles) at 37°C before (open circles) and after (shaded squares) a temperature cycle down to 25°C. The consistency of the measurements emphasizes the reproducibility of the polymer-bilayer structures. (b) NR data from PNIPAAm-co-MaBP in D2O at 37°C. The NR data of the polymer are depicted before depositing DPPE (open circles) and after removing DPPE but before depositing DPPC (shaded squares). The consistency of the measurements shows that the polymer structure was unaltered by depositing or removing DPPE. Error bars indicate 1 SD.