Skip to main content
. 2011 Jun 22;2011:836587. doi: 10.1155/2011/836587

Figure 10.

Figure 10

Relationship between tensile strength and elongation of TNTZ added with Y2O3 (0.05YCR: TNTZ-0.05YCR, 0.1YCR: TNTZ-0.1YCR, 0.2YCR: TNTZ-0.2YCR, 0.5YCR: TNTZ-0.5YCR, and 1.0YCR: TNTZ-1.0YCR) and TNTZ subjected to severe cold rolling after solution treatment (TNTZCR).