Table 2.
Mechanical and morphological parameters of the four models and experimental findings utilizing postmortem retrievals (Miller et al., 2010; Miller et al., 2011). Unfortunately, no experimental postmortem retrieval data in pure shear was available
| Model | 0° | 0° | 180° | 90° | CI [−] | II [−] | GT [mm] |
|---|---|---|---|---|---|---|---|
| T N,ult [MPa] | |||||||
| 1 | 0.55 | 21.7 | 248.1 | 154.4 | 0.18 | 1.01 | 0.101 |
| 2 | 0.10 | 5.4 | 21.4 | 10.1 | 0.13 | 1.34 | 0.231 |
| 3 | 0.81 | 93.0 | 258.6 | 139.4 | 0.29 | 1.26 | 0.076 |
| 4 | 0.56 | 37.7 | 441.2 | 184.3 | 0.74 | 1.20 | 0.015 |
|
| |||||||
| Mean (SD) | 0.51 (0.30) | 39.5 (38.1) | 242.3 (171.9) | 122.1 (76.9) | 0.34 (0.28) | 1.20 (0.14) | 0.11 (0.09) |
|
| |||||||
| Miller et al., 2010 Mean (SD) |
0.21 (0.32) | 16 (35) | 47 (61) | - | 0.11 (0.17) | 0.72 (0.62) | 0.33 (0.28) |
|
| |||||||
| Miller et al. 2011 Mean (SD) |
- | 19.2 (25.6) | 22.7 (35.7) | - | 0.57 (0.31) | 1.89 (0.69) | - |