Skip to main content
. 2011 Feb 4;2:85–98. doi: 10.3762/bjnano.2.10

Figure 10.

Figure 10

Logarithm of the dissipated power in moving as-synthesized NPs on silicon wafer versus the tip scan speed. Substrates: circles: SiO2 silicon wafer; squares: NH2-coated silicon wafer (hydrophilic substrate); triangles: CH3-coated silicon wafer (hydrophobic substrate). (a) 35 nm diameter Au NPs, (b) 60 nm diameter Au NPs.