Figure 5.

Figure 5

The development of polymerization stresses measured using the newly designed tensometer as a function of sample position for different sample heights (hs). The error bars indicate the standard deviation of the measurement, which is a Type A standard uncertainty. The lines are best fit for the corresponding data. The stress was obtained at 1 hr after irradiation.