Skip to main content
. Author manuscript; available in PMC: 2012 Aug 18.
Published in final edited form as: Polymer (Guildf). 2011 Aug 18;52(18):3887–3896. doi: 10.1016/j.polymer.2011.07.007

Figure 3.

Figure 3

The effect of UV initiator concentration on shear storage modulus of SPELGA5K-L100-M25-N0 hydrogels. The intensity, distance from the sample, and exposure time of the UV radiation were 46,000 µW/cm2, 10 cm, and 1800 s, respectively. Values are the mean of three samples with error bars representing one standard deviation from the mean.