Published in final edited form as: Polymer (Guildf). 2011 Aug 18;52(18):3887–3896. doi: 10.1016/j.polymer.2011.07.007

Figure 6.

Figure 6

The effect of initiator molecular weight and LA/GL ratio of SPELGA macromonomer on shear storage modulus of SPELGA-M15-N0-I0.16 hydrogels. The intensity, distance from the sample, and exposure time of the UV radiation were 46,000 µW/cm2, 10 cm, and 1800 s, respectively. Values are the mean of three samples with error bars representing one standard deviation from the mean.