. 2010 May 25;15(5):625–633. doi: 10.1007/s00784-010-0426-6

Fig. 2.

Fig. 2

a–c Changes in repair bond strengths with respect to non-aged controls for the four composite resins involved in this study, following conditioning using either IAR- or SC-application and after a thermocycling, b water storage, and c citric acid immersion. Error bars denote the SD over ten different specimens per group