Table 2.
Failure load (N) | Stiffness (N/mm) | Work to failure (N.mm) | ||||
---|---|---|---|---|---|---|
Initial | 2615 ± 1136 | (651–5481) | 2938 ± 1585 | (663–6741) | 1730 ± 1129 | (453–4158) |
Postfracture | 2285* ± 970 | (566–4547) | 1277* ± 596 | (156–2357) | 3219* ± 1745 | (654–7524) |
Δ (%) | −11 ± 19 | (−53–21) | −53 ± 18 | (−76 to −2) | 121 ± 104 | (−34–425) |
Note: Δ = difference between postfracture and initial parameters in % [mean ± SD (range)]. The comparisons between initial and postfracture mechanical parameters were performed using Wilcoxon signed-rank tests (*p < .05).