Table 1.

Summary of properties of the 4000E and 5000E TM phantoms.

Quantity 4000E TM phantom 5000E TM phantom
Bead concentration (g∕l) 6.00 15.60
Mean bead diameter (µm) 5.40 5.16
Thin layer covering TPX Saran wrap
Density (g∕ml) 1.045 1.062
Speed of sound (m∕s) 1541 1541
Atten. α0 (dB∕cm) 0.107 0.069
Atten. n 1.52 1.66
BSC at 30 MHz (sr−1cm−1) 0.040 0.130