Skip to main content
. 2009 Aug 27;15(4):477–484. doi: 10.1089/ten.teb.2009.0340

FIG. 1.

FIG. 1.

Effects of dynamic loading on the mechanical properties of cartilage contstructs.1 Mechanical preconditioning was carried out with three intermittent (separated by 1 h) loading cycles per day of 10% deformation at 1 Hz. Loading was then carried out for 5 days per week for a total of 4 weeks. *, Indicates significant differences between loaded samples and free-swelling controls; **, indicates a significant difference between peak stress of day 21 and day 28 loaded samples.