Plot of carbon loading (% C, w/w) vs. CVD time for alumina (◇), 8 μmolAl/SiO2 (Δ) and 2 μmolAl/SiO2 (○). The arrow is to help compare induction times between 8 μmolAl/SiO2 and 2 μmolAl/SiO2. CVD temperature is 700 °C for all data.