Fig. 16.

Fig. 16

Effect of hypercrosslinking of poly(styrene-co-chloromethylstyrene-co-divinylbenzene) precursor monolith on the specific surface area. Conditions: Polymerization mixture used for the preparation of precursor monolith: 16% styrene + chloromethylstyrene, 24% divinylbenzene, 18% toluene, 42% 1-dodecanol, 1% (with respect to monomers) azobisisobutyronitrile; hypercrosslinking 24 h at 80°C. Reproduced from ref. [64].