Integral pore size distribution profiles of poly(styrene-co-divinylbenzene) monoliths prepared by a polymerization at different temperatures. Conditions: (A) polymerization mixture styrene 20 wt%, divinylbenzene 20 wt%, 1-dodecanol 40 wt%, toluene 20 wt%, benzoyl peroxide 0.5 wt% (with respect to monomers), temperature 70 °C, reaction time 24 h; (B) polymerization mixture styrene 20 wt%, divinylbenzene 20 wt%, 1-dodecanol 60 wt%, benzoyl peroxide 0.5 wt% (with respect to monomers), temperature 130 °C, reaction time 8 h.