. 2011 Feb 25;6(1):176. doi: 10.1186/1556-276X-6-176

Table 1.

FE parameters of Au film-coated SiNWs with different thicknesses

Samples Eon, (V/μm) EJ = 100μA/cm2 (V/μm) Φ (eV)
As-grown SiNWs 5.01 5.93 4.15
Au20/SiNWs 6.02 7.20 4.29
Au60/SiNWs 6.03 7.81 4.51
Au80/SiNWs 7.51 9.18 4.98
Au - - 5.55