InGaN/GaN multiple QW |
463 |
Ag |
Transmittance exhibits absorption from 396 to 455 nm |
32.2% with an 100-mA current |
Kwon et al. [33] |
Alq3 thin film |
525 |
Au |
A peak in absorption at 510 nm |
20-fold |
Fujiki et al. [34] |
InGaN/GaN QW |
550 |
Ag |
A dip in transmission at about 550 nm |
150% in peak intensity with a 20-mA current |
Yeh et al. [36] |
InGaN/GaN QW |
465 |
Au |
A dip in transmission in 511 nm |
180% with a 20-mA current |
Sung et al. [37] |
Organic poly |
575 |
Ag |
Large absorption from 330 to 500 nm |
Sixfold |
Qiu et al. [41] |
Si QD |
600 |
Ag |
A peak in absorption at 535 nm |
Reaches maximum at 530 nm |
Kim et al. [42] |
ZnMgO alloys |
357 |
Pt |
Extinction band near 350 nm |
Sixfold |
You et al. [44] |
ZnO film |
380 |
Ag |
Extinction band near 370 nm |
Threefold |
Cheng et al. [45] |
Si-on-insulator |
1,140 |
Ag |
A dip in transmission at about 520 nm |
2.5-fold in peak intensity |
Pillai et al. [48] |
CdSe/ZnS nanocrystals |
580 |
Au |
A peak in absorption at about 600 nm |
30-fold |
Pompa et al. [53] |
Si QD |
775 |
Ag |
A dip in transmission at 710 nm |
Twofold, with the peak blue shifts |
Biteen et al. [54] |
GaN |
440 |
Ag |
A dip in transmission at about 440 nm |
Twofold |
Mak et al. [62] |